Nickel Alloy Bar/Rod

PRODUCTS

‹

›

GH536/GH586/GH605/GH648/GH901 Nickel-based superalloy Rod/Bar Chinese Manufacturer

Grade: GH536/GH586/GH605/GH648/GH901
Available Standard: ASTM, EN, JIS, GB, etc.
Delivery time: Within 15 days, or upon negotiation
Terms of price: EXW, FOB, CFR, CIF
Payment Term:TT etc
Certificates: SGS MTC ISO9001 CE SGS

If you have any questions, please feel free to contact us.

Ask for a quote

PRODUCT  INTRODUCTION


Nickel will alloy readily with many other metals, including chromium, iron, molybdenum and copper. This allows for a wide variety of alloys that demonstrate outstanding resistance to corrosion and high-temperature scaling, exceptional high-temperature strength and other unique properties, such as shape memory and low coefficient of expansion.


The following is a simplistic categorisation of the various nickel alloy types.


Wrought Nickel


Pure nickel UNS N02200 is used in the chemical industry for its corrosion resistance - particularly to alkalis. It is also used for its properties in shielding against electromagnetic interference and in transducers.


Nickel-Iron Alloys


These are used as soft magnetic materials, as glass-to-metal seals and as materials with defined thermal expansion properties.

Invar® (UNS K93600), with 36% nickel and the remainder iron, is unique in having an almost zero coefficient of thermal expansion around room temperature. This makes it valuable where high dimensional stability is required, such as in precision measuring instruments and thermostat rods. It is also used at cryogenic temperatures because of its very low thermal expansion rates.

Alloys containing 72-83% nickel have the best soft magnetic properties and are used in transformers, inductors, magnetic amplifiers, magnetic shields and memory storage devices.


Nickel-Copper Alloys


These are highly resistant to corrosion by alkaline solutions, non-oxidizing salts and seawater. The best-known is Alloy 400.


Nickel-Molybdenum Alloys


These are highly resistant to reducing acids in the absence of oxidizing ions, such as ferric and cupric or dissolved oxygen. The best-known is Alloy B-2.


Nickel-Chromium Alloys


These are characterised by their high resistance to corrosion at both normal and high temperatures (resistance to scaling), good high-temperature strength and high electrical resistance. There are three main groups of alloys:


·Ni-Cr (and also Ni-Cr-Fe) alloys with high electrical resistance for heating elements, such as 70-30 (UNS N06008) and C-Grade (UNS N06004)

·Ni-Cr alloys (with Fe and other alloying elements) with good corrosion resistance. The best-known are Alloy 600 (UNS N06600) and Alloy 601 (UNS N06601)

·Ni-Cr alloys with high-temperature strength and creep resistance, mostly age-hardenable, such as Alloy X-750 (UNS N07750)



Nickel Alloy Bar Description



Product nameNickel Alloy Bar/Rod
Diameter5-600mm or as required
ServiceCutting( laser catting, plasm cutting, cutting machine) forged produce
Standard
AISI, ASTM, DIN, EN, GB, JIS
InspectionISO, BV,SGS, MTC
Treatment processNickel electroplating, heat treatment, chemical treatment, alloying, etc
Mainly grade

ASTM grade: Incoloy 800/800H, Incoloy825, Inconel600, Inconel 625, Inconel690,

Hastelloy B, Hastelloy B-2, Hastelloy276, Hastelloy C4, Hastelloy C2000.

ASME grade: N08800, N08810, N08825, N06600, N06601, N06690, N10001, N10665, N10276, N06455, N06625

EN grade: 1.4588, 2.4858, 2.4817, 2.4642, 2.4617, 2.4819, 2.4612, 2.4856

Application

Widely used in petroleum, foodstuff, chemical industry, construction, electric power,nuclear

energy, machinery, biotechnology, paper making, shipbuilding, boiler fields

MOQ1 ton
Delivery timeWithin 7-15 working days.
Export packing
Standard export packing or according to the customers' request.
Capacity5000+tons/Month



Nominal composition of various nickel alloys:



Alloy nameUNS% Ni% Cr% Fe% Mo% Cu% Co% Other
200N0220099 min





InvarK9360036
64



400N044006532




B-2N1066568
228


70-30N060087030




C-GradeN060066016bal



600N0660076168



601N066016023bal


Al - 1.3
X-750N0775070157


Ti - 2.5Al - 0.7Nb - 1.0
825N0882542212532

G-3N06985bal222072

800N08800322145


W - 3.5
C-276N10276bal15516


C-22N06022bal21413


59N06059bal231.5 max16


C-2000N06200bal233 max161.6

686N06686bal212 max16

W - 3.7
617N0661744.5 min223 max9
12
HR-160N12160bal283.5 max

30Si - 2.75
NitinolN0155555




Ti - 45



Nominal composition of various nickel alloys:



Alloy TypeUNS%Cr%Ni%Mo%Cu%Fe
304LS30403188--balMost common stainless steel used for potable water treatment and food contact.
316LS3160316102.1-balAddition of Mo provides greater resistance to chlorides and acidic solutions. Used in coastal regions, in water treatment and in the chemical processing industry.
2205S32205225.73.1-balEven greater corrosion resistance than 316L. Can be used in place of 316L, but its greater strength can mean weight reduction. May be  substituted for 316L if it fails in service.
2507S327502574-balEven greater corrosion resistance than 2205. Useful corrosion resistance to seawater.
254 SMOS3125420186.1-balCorrosion resistance similar to 2507, also possessing useful corrosion resistance to seawater.
Alloy 20N0802020332.13.2balCu bearing stainless steel with useful corrosion resistance to all concentrations of sulphuric acid.
310SS310082520--balHigh chromium stainless steel with excellent resistance to high-temperature oxidation.
800HN088102032--balStainless steel with excellent high-temperature strength and useful resistance to high-temperature oxidation.
625N0662521bal9-3Well-known nickel alloy with excellent high-temperature strength and outstanding aqueous corrosion resistance.
C-276N1027615bal16-5One of the best-known nickel alloys with excellent corrosion resistance to reducing acids.
600N066001676--8Useful resistance to high-temperature corrosion and caustic solutions.
Alloy 400N04400-65-32-Most common uses are in marine and chemical processing.



PRODUCT  DISPLAY

workshop.jpg

PACKAGING

PACKAGING.jpg

WHY CHOOSE US

Lianyungang Dapu Metal Co.,Ltd has been engaged in the steel industry for over 15 years as well as rich steel experience in both the international market, and domestic market. The company has standard workshops and modern comprehensive equipment, providing a strong guarantee for high-quality products. The company has established strategic partnerships for import and export business with many famous enterprises. Now more than 10,000 tons of inventory and over 800 specifications in stock so that can ship timely to meet clients demand. These products are suitable for engineering, coal, textile, electric power and other industries.

LIANYUNGANG DAPU METAL CO.,LTD
LIANYUNGANG DAPU METAL CO.,LTD

Adequate supply

Adequate stock of various products, ready to place orders and ship at any time.

Quality promise

Provide return and exchange service for customers. Provide email and phone inquiries throughout the product transaction.

Competitive Price

We can provide competitive price, please contact us for quotation.

Deliver Faster

Arrange production immediately upon receipt of advance payment within 24 hours We can make transportation plan according to your requirements.

LEAVE A MESSAGE

Submit

RECOMMENDED PRODUCTS